TECHNET Archives

November 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"COLLINS, GRAHAM" <[log in to unmask]>
Reply To:
TechNet Mail Forum.
Date:
Mon, 17 Nov 1997 14:22:21 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (67 lines)
Ken
We do it monthly, but are considering changing to an hours run period
(add a hour meter to the circuit for the wave pump).  The things you
need to consider are:
- how much volume is run through the machine (number of shifts / boards
per shift)
- complexity / size (ie. 100 PCMCIA cards would contaminate differently
than 100 cards that measure 15" x 20")
- history - what have your samples found in the past, trends, recent
maintenance activity...

As is usual on this forum, opinions are mine and worth what you paid for
them.

regards,

Graham Collins
Process Engineer,
Litton Systems Canada Limited
(902) 873-2000 ext 215
> -----Original Message-----
> From: Ken Patel [SMTP:[log in to unmask]]
> Sent: Monday, November 17, 1997 3:04 PM
> To:   [log in to unmask]
> Subject:      [TN] frequency of solder pot content analysis
>
> Wave Expert,
>
> How often one should take solder sample from the wave solder pot for
> content
> analysis (impurities)? Is there a guideline which assembly house
> should follow?
>
> re,
> ken patel
> ______________________________________________________
> Ken Patel                       Phone:  (408) 490-6804
> 575 Cottonwood Dr.              Fax:    (408) 490-6859
> Milpitas, CA 95035              Beeper: (888) 769-1808
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
> 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2