A week or so ago, there was a posting on whether hand soldering equipment will need to be changed to handle lead free solder. The only hand solder iron mentioned was a Metcal, and I am wondering if anyone out there is using Wellers?
We use Weller Irons with 700 degree tips. Any advice is welcome.
Thanks
Marie
Marie A. Dobbs
Training and Development Specialist
Tyco Safety Products
100 Technology Drive
Westminster, MA 01473
Phone: 1-978-731-6827
Fax: 1-978-731-6950
email: [log in to unmask]
In any moment of decision the best thing you can do is the right thing, the next best thing is the wrong thing, and the worst thing you can do is nothing."
Theodore Roosevelt
26th President of the United States
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|