check the warping of the BGA PWB carrier pre and post reflow.... as the PWB
warps, it may be pushing the solder...another check point may be your stencil
design/process....
Marcelo
-----Original Message-----
From: Poh Kong Hui [SMTP:[log in to unmask]]
Sent: Thursday, December 10, 1998 10:07 AM
To: [log in to unmask]
Subject: [TN] BGA short
Hi Technetters,
I am facing a weird problem.
One of the board that we make, is having short underneath the BGA.
However, every single short is always at one of the 4 corners of
the BGA.
Is there anyone facing such an issue ? Could someone advise me how
to solve.
Poh
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|