Steve,
Our customers who use their products in extreme conditions demand
silicone coating. They rely on the moisture resistance. Besides, it is
easy to validate the coating with uv lighting.
Eric
-----Message d'origine-----
De : TechNet [mailto:[log in to unmask]] De la part de Steve Gregory
Envoyé : 4 septembre, 2003 15:35
À : [log in to unmask]
Objet : [TN] Silicone conformal coating
Hi All!
I know when you look up properties for Silicone conformal coating, it
usually states that it has good moisture resistance, but is it really
that good?
I've heard that it is somewhat permeable to moisture, that if you were
worried about moisture, and the assembly were going to see the outside
environment, you would be better off with an acrylic, or urethane
coating.
Any thoughts?
Thanks!
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|