TECHNET Archives

April 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 16 Apr 2010 10:33:32 -0700
Reply-To:
Subject:
From:
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; format=flowed; charset="iso-8859-1"; reply-type=original
MIME-Version:
1.0
Parts/Attachments:
text/plain (64 lines)
We have found a factor that is not to be found in any standard or paper, 
namely, the size of the components. If you  have e.g. a mobile telephone 
card,  all components are the tiniest that are to be found on the market. 
With that follow extremly small solder pads equal to extremly small solder 
volumes.  Such card are more sensitive to  solder tarnish than board with 
much bigger components. Therefore, Ericsson have a storage  maximum of a 
couple of weeks only. I  have never seen a investigation of that condition. 
Nor any calculations or rules.

Inge

--------------------------------------------------
From: "Bill Belanger" <[log in to unmask]>
Sent: den 16 April 2010 10:14
To: <[log in to unmask]>
Subject: Re: [TN] PCB Shelf life

> Hello Angel,
>
> As a former PCB fabricator, I'm not sure that the base material has a 
> shelf
> life. It's usually quite stable, and lasts a very long time in the field.
>
> Solderability, however, is a different story. Some surface finishes can
> preserve solderability for many years, such as HASL (Hot Air Solder 
> Level),
> which essentially coats any exposed copper with solder. Others, such as
> immersion tin and OSP (Organic Solderability Preservative), measure their
> shelf life in months, weeks or days.
>
> Hope this helps,
>
> Bill Belanger
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815
> -----------------------------------------------------  


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2