Try Hamilton precision Metals in Lancaster PA USA, (Sorry I don;t have
the address handy)
Or Goodfellow there in the UK (44(0)1223568 068
----------
From: Colin
To: [log in to unmask]
Subject: [TN] Nickel foil
Date: Thursday, May 28, 1998 11:16AM
Fellow Technetters,
I have had a request from one of my UK customers, where it would be
possible to source FULLY ANNEALED nickel foil.
He is looking for 18uM thick foil, treated preferably on both sides, but
one will suffice, in panel sizes around 18" x 12" or 24" x 18".
Any leads as to where I might get this material, either in Europe or
Stateside?
Either reply via TechNet, or off-line.
Thanks in advance.
Colin McVean
Polyclad Technical Services UK
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|