TECHNET Archives

July 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stephen R. Mikell" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 16 Jul 1998 15:19:17 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (36 lines)
Hello,

I am looking for a tinning service to deal with an SMT part best described as
a ceramic SOJ-36.  The part has side brazed, gold plated J-leads.  The service
should have extensive experience tinning SMT devices and dealing with
coplanarity issues arising from uneven solder deposits during tinning.  Any
offers or recommendations are welcome, on-line or off-line.  Additional
details below for those interested.

Steve Mikell
SCI Systems Plant 13
(256)-882-4800 x9366
[log in to unmask]

Problems
1. The metalization of the part extends onto the bottom of the part body.  The
end of the J-lead curls to within 0.010" of the bottom of the part.  Per spec
we need to remove the gold plating from the to be soldered surface, but we
also need to not kill the what little stress relief this design offers by
soldering the lead to the part bottom.
2. Coplanarity of the lead bottoms must not exceed a range of 0.005".  A small
blob of solder on the bottom of one lead may raise other leads out of the
solder paste, resulting in solder defects.

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2