Hi Blair
What soldering processes? We run two selective solder machines using a nitrogen generator, it is reasonably economical. And pretty low maintenance. At a previous job I looked at replacing the liquid nitrogen tank with a generator, big bucks but so is tank nitrogen.
cheers,
Graham Collins
________________________________________
From: TechNet [[log in to unmask]] on behalf of Blair Hogg [[log in to unmask]]
Sent: Wednesday, January 10, 2018 12:56 PM
To: [log in to unmask]
Subject: [TN] Nitrogen generators
Hi Technetters,
We are thinking of switching from using bottled / tanked nitrogen for our soldering processes to getting a nitrogen generator. Looking for advice on what systems others are using and what they like / dislike about them. You can reply directly if you don't want to share with the list.
Thanks,
Blair