TECHNET Archives

January 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Bissonnette, Jean-Francois" <[log in to unmask]>
Date:
Thu, 11 Jan 2001 13:22:22 -0500
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Bissonnette, Jean-Francois" <[log in to unmask]>
Parts/Attachments:
text/plain (94 lines)
Hi Bob,

Thank you for the detailed explanation.

You talk about a "quick-check hole diameter validation area"
my question is can you rely on these at incoming inspection?
Or should a sample check be done on a number of boards?

Thanks!

JF

BTW:  Thanks to everyone for your answers, that's a lot of
help!


> -----Original Message-----
> From: Robert Lazzara [mailto:[log in to unmask]]
> Sent: Wednesday, January 10, 2001 1:50 PM
> To: [log in to unmask]
> Subject: Re: [TN] PWB hole size verification
>
>
> In a message dated 1/10/01 1:17:38 PM Eastern Standard Time,
> [log in to unmask] writes:
>
> << What is the method used for verifying that the hole sizes
> of the production
>  board have the required size??? >>
>
> Jean-Francois,
>
> Pin gages are simple to use, have excellent tolerancing and
> are solid-state
> stable. Pin gages do require a bit of technique, however, as
> the operator can
> influence a "fit" in marginal situations (pass me the hammer).
>
> Pins may also inadvertently remove burrs and other
> diameter-influencing
> protrusions that might not be displaced by component leads,
> possibly giving a
> better-than-deserved indication.
>
> Pin gauging should sample the PCB from both high and low
> circuit density
> areas, as the rate of electroplating deposit (and subsequent
> hole diameter)
> will vary.
>
> If your boards are received in an array or pallet, you might
> consider having
> the fabricator drill a series of holes, 1-each of the applied
> sizes, in a
> sequence of descending order in the assembly rails. This can
> be subsequently
> used as a quick-check hole diameter validation area.
>
> Bob Lazzara
> Circuit Connect, Inc.
>
> --------------------------------------------------------------
> -------------------
> Technet Mail List provided as a free service by IPC using
> LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with
> following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following
> message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources
> & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm)
> for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> --------------------------------------------------------------
> -------------------
>


WABTEC CORPORATION CONFIDENTIALITY NOTE
The content contained in this e-mail transmission is legally privileged and confidential information intended only for the use of the individual or entity named herein. If the reader of this transmission is not the intended recipient, you are hereby notified that any dissemination, distribution, or copying of this transmission is strictly prohibited.

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2