I couldn't find our copy of 7721 but I have done this mod. several times. We did not add a pad. So long as the part is bonded I see no real benifit to adding one other than you could then attach the wire there instead of the part which some people may want for aesthetics. The last time I added a pad for a mod. I also added traces.
Charles Caswell

-----Original Message-----
From: [log in to unmask]
[mailto:[log in to unmask]]
Sent: Tuesday, July 15, 2003 10:30 AM
To: [log in to unmask]
Subject: [TN] Surface mount diode-no pad one end


    I have an engineering modification proposal which has a surface mount diode
shifted so that only one end is on an original solder pad. The other end will
have a wire soldered to the terminal which has no PWB solder pad. The component
body will be bonded to the board.

    It has been past practice in this Class 3 and MIL-STD house to add a pad for
the modification but that is coming under question now. My research has not
turned up a requirement or a guideline to show that a pad is required. IPC R-700
and 7721 do not address this situation. Does anyone know of a paragraph to
provide guidance?

Thanks,

Stu Korringa
Smiths Aerospace
Grand Rapids, Michigan
[log in to unmask]
616.241.8189


**********************************************************************
This e-mail and any files transmitted with it may be confidential and
may be legally privileged or otherwise exempt from disclosure under
applicable law. This e-mail and its files are intended solely for
the individual or entity to whom they are addressed and their content
is the property of Smiths Aerospace.  If you are not the intended
recipient, please do not read, copy, use or disclose this communication.
If you have received this e-mail in error please notify the e-mail
administrator at [log in to unmask] and then delete this
e-mail, its files and any copies.

This footnote also confirms that this e-mail message has been scanned
for the presence of known computer viruses.

Smiths addresses are changing!  The new addresses are of the form
[log in to unmask]  Please update your address
books!  Please begin using the new form immediately.
***********************************************************************

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2