Our friends at Rockwell have a chart in one of their presentations that show
CTE of various common laminates up to a typical reflow temp.
At room temp CTE of them is about 25ppm /degree C. But, by 150 C things get
less predictable. And can be 75 ppm / degree.
The thing is you are trying to attach a flex. What is its CTE. The
difference between the two? It is important.
Part two of your question The Z axis expansion of the woven substrate will
be higher than the "x-y" advertized CTE. So, no I would not expect the
material to shrink. What happens of the flex expands wildly above 100 C, you
might think the substrate shrank . . .
Guy
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Eric Christison
Sent: Friday, July 02, 2010 11:12 AM
To: [log in to unmask]
Subject: [TN] Question about FR4 Curing
I'm wondering about an issue we have with the dimensional stability of a
substrate made of FR4.
We're finding it's deforming during a flex attach operation, not by much
but enough to cause us a problem. We use ACF and a hot bar. The
substrate sees a temperature of 155 deg C for about 10 seconds. Someone
suggested that the movement may be due to incomplete curing of the
substrate.
I'm wondering if a temperature of 150 deg C for 10 seconds is likley to
have any effect at all on the matrix.
If it did, would the volume of the matrix increase, decrease or stay
much the same?
I realise that we'll see deformation due the application of pressure as
well but in some instances the substrate seems to be moving in the wrong
direction.
Thanks,
--
Eric Christison
Consumer& Micro group
Imaging Division
STMicroelectronics (R&D) Ltd
33 Pinkhill
Edinburgh EH12 7BF
United Kingdom
Tel: +44 (0)131 336 6165
Fax: + 44 (0)131 336 6001
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|