Sandra,
Try Loctite Prism 454 adhesive. This is made for tacking thermocouple
wires onto pc boards for running profiles.
Bruce Adams
Datametrics Corp.
Orlando, FL 32809
[log in to unmask]
> -----Original Message-----
> From: Sandra Davis [SMTP:[log in to unmask]]
> Sent: Thursday, April 15, 1999 8:45 PM
> To: [log in to unmask]
> Subject: [TN] Thermocouples on Hard Drives
>
> Does anyone have any suggestions on how to best measure temperature of
> hard
> drive critical components?
>
> I am working from a more macro level, assembling hard drives into
> swappable
> sleds in electronic enclosures. Enclosure design may or may not be
> providing sufficient air flow past the hard drive HDA, and other chips
> commonly identified as U14, U5, etc.
>
> I am duct-taping stiff thermocouple wires onto the chip outer
> surfaces, and
> flipping the drive over and mounting it onto a sled (the thermocouples
> and
> exposed chips are wrapped by my metal sled). I'm then taking the
> other end
> of the wires, and with K connections, using a Fluke 52.
>
> Duct tape is horrendous for a thousand reasons.
> Adhesive with activator won't hold the stiff wire tip in place long
> enough
> to cure.
> I'm looking into thermocouple wires with self-adhesive tabs.
>
> Any added suggestions I'd greatly appreciate.
>
> Thank you,
> Sandra Davis
>
> Sandra R. Davis, Mechanical Engineer
> Artecon, Inc., 6305 El Camino Real, Carlsbad, CA 92009
> Phone: (760) 931-5507, Fax: (760) 931-5527
> email: [log in to unmask], URL: http://www.artecon.com
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|