>Richard,
Check with Electrovert, they used to put on a school for wavesoldering.
Larry Tawyea
Thank you all for your responses about this issue. Main points were:
> - temperature (too high or too low)
> - flux activity
> - contact time
> - possible shadowing
> - clealiness of the pads
> - diffused nickel
> - turbulence
>
>I still haven't checked all that though.
>
>Does anybody know about a good course/tutorial for engineers about wave
>soldering ? I need it.
>I checked with IPC, EMPF and SMTA and I didn't see anything in a near
>future.
>Thank you.
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
>following text in the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
>additional information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>847-509-9700 ext.311
>##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|