TECHNET Archives

October 2018

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 19 Oct 2018 13:55:41 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Yuan-chia Joyce Koo <[log in to unmask]>
Message-ID:
Subject:
From:
Yuan-chia Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"; delsp=yes; format=flowed
MIME-Version:
1.0 (Apple Message framework v753.1)
Parts/Attachments:
text/plain (16 lines)
plating condition got a lot to do with hardness, not just alloy...  
(additive too - such as brightener, for example).
ps.  I can see the weather is very good for golf in your neck of  
goods - we are ready for snow...;-(.
jk
On Oct 19, 2018, at 1:10 PM, <[log in to unmask]>  
<[log in to unmask]> wrote:

> Fellow TechNetters:
>
>    Are there any papers/studies out there that provides insight  
> into the golf hardness formulation by specifics alloys, Gold,  
> Copper, Silver, Nickel, Palladium, Zinc, Rhodium and platinum.
>
> Victor,