TECHNET Archives

October 2011

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Bob Landman <[log in to unmask]>
Date:
Mon, 3 Oct 2011 04:25:35 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Inge Hernefjord <[log in to unmask]>
Subject:
From:
Inge Hernefjord <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="ISO-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (97 lines)
If that pedal accelerates tin whiskers, you may retard the growth by using
the brake pedal.
American logic.
/Inge
PS. I'm afraid I just trigged Dewey. Let's see if he can resist.

2011/10/2 Bob Landman <[log in to unmask]>

> Some of us here attended the 5th CALCE  international symposium on tin
> whiskers http://www.calce.umd.edu/symposiums/ISTW2011.htm where one  of my
> former professors, Dr. Henning  Leidecker, talked about the tin whiskers he
> and the others at NASA Goddard  discovered in Toyota Camry accelerator
> pedals.
> =====================================
> CALCE Prediction of Potential Failures Risks in Toyota  Vehicles Confirmed
> by NASA Scientists
> Investigations of Toyota vehicles have revealed tin whiskers in a critical
>  component of their vehicle engine control system. At the September CALCE
>  Conference on Tin Whiskers, Henning Leidecker and his team at NASA's
> Goddard  Space Flight Center, who are recognized experts on electronic
> device failure and  tin whiskers, presented their studies of tin whiskers on
> Toyota vehicles. They  determined that the risk of failure due to tin
> whisker shorting in affected  Toyota vehicles can be on the order of 50 to
> 150 per million. This figure agrees  with the number reported in a recently
> published scientific journal article  [Sood et al.] written by CALCE
> researchers Bhanu Sood, Michael Osterman, and  Michael Pecht. They assessed
> the probability of a tin whisker-induced electrical  short to be 140 per 1
> million, based on whisker growth statistics.
> Tin whiskers are known to grow from tin-finished surfaces and have been
>  associated with costly failures of electronic systems. Linking tin whiskers
> to  electronic product failure is often extremely difficult. Tin whiskers
> that  bridge across terminations can create electrically resistive pathways.
> And since  whiskers shift under an electrostatic field and can melt when the
> electrical  current is drawn, they cause intermittent electrical behavior in
> systems.
> Figure 1 Tin whiskers on the edge of an acceleration position sensor board
>  connection terminal in a 2002 Toyota Camry.
>
> http://www.autosafety.org/sites/default/files/imce_staff_uploads/whisker%20news%20article-update-review%20%282%29.pdf
> Considering the number of vehicles on the  road, the presence of tin
> whiskers in engine control components presents a  significant safety hazard.
> For this reason, best practices for electronics  design stipulate that tin
> not be used as a plating material. It is very  questionable why the National
> Highway Traffic Safety Administration--with its  stated mission to --save
> lives, prevent injuries and reduce economic costs due to  road traffic
> crashes, through education, research, safety standards, and  enforcement
> activity||--has not come out with a requirement that no electronics  use pure
> tin as a material component, since the potential for tin whiskers  presents
> an unreasonable and unnecessary risk.
> B. Sood, M. Osterman and M. Pecht,  Tin Whisker Analysis of Toyota's
>  Electronic Throttle Controls, Circuit  World, Vol. 37, No. 3, 2011, pp. 4-9
> =====================================================
>
> (One of my colleagues,  Dr. Gordon Davy, presented a talk on our process:
>  "Whisker-Impenetrable Metal Cap Process for Electronic Assemblies"  )
>
> Bob Landman
> Managing  Partner
> LDF  Coatings, LLC.
> [log in to unmask]
> www.ldfcoatings.com
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2