TECHNET Archives

February 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 25 Feb 2000 23:52:32 EST
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
"Dr. Jerome S Sallo" <[log in to unmask]>
Parts/Attachments:
text/plain (26 lines)
Hans
One cannot conclude with certanty that the lower Tg material is the prepreg.
Since the core has been through two lamination cycles (at the laminator and
in your press) it is usual to infer that the lower Tg is the prepreg. This is
reinforced by the single peak after heating. One material or the other was
undercured after your lamination cycle. Did the second lab you mentioned heat
the material after DSC as much as the first lab to complete the cure?  If
these data represent real boards I suggest a bake to fully cure them. Hard
top be sure, these are thoughts which I hope will help
Jerry Sallo
Sallo Consulting Services

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2