Hi all,
Just a reminder that the solder at those pins are most
likely high temp solder; otherwise this part could not
be processed with wave soldering.
Ted
--- "Croslin, Robert"
<[log in to unmask]> wrote:
> Dann, we've done more than our share of these as our
> stuff gets built for 20
> - 25 years and obsolescence is an issue, but what
> we've used for pins are
> strip style headers on .10 centers. That way, it
> all fits within normal
> processes. In looking at your picture, it almost
> looks like the pins may
> have been on a band that was broken away after they
> were soldered. It would
> almost certainly have to be fixture to hold
> alignment, but this is the first
> time I've seen those pins. Any chance you could use
> a strip header? You do
> have to watch the height, though.
>
> Bob Croslin
> Nielsen Media Research
>
>
> -----Original Message-----
> From: d. terstegge
> [mailto:[log in to unmask]]
> Sent: Friday, November 14, 2003 9:01 AM
> To: [log in to unmask]
> Subject: [TN] Replacing a DIP package
>
>
> Hi Technet,
>
>
http://www.parallax.com/images/prod_jpg/bs2p24-ic.jpg
> is a picture of a
> tiny pcb assembly that can be wavesoldered onto a
> motherboard almost
> like a normal through-hole package. Due to an
> obsolescense problem we
> are thinking about replacing a 22-pins DIP-package
> by a construction
> similar to what's in the picture.
> Does anyone know what technology to use to get the
> sidepins connected
> to the substrate, and does this fit within a normal
> PCB Assembly
> process? Also any ideas about alternative solution
> are more then
> welcome.
>
> Best regards!
>
> Daan Terstegge
> Thales Communications
> Unclassified mail
> Personal Website: http://www.smtinfo.net
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using
> LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask]
> with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of
> Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts:
> send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach
> Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
>
-----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using
> LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask]
> with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of
> Technet send e-mail to [log in to unmask]: SET Technet
> NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts:
> send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-509-9700 ext.5315
>
-----------------------------------------------------
__________________________________
Do you Yahoo!?
Protect your identity with Yahoo! Mail AddressGuard
http://antispam.yahoo.com/whatsnewfree
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|