TECHNET Archives

October 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Daniel Blass <[log in to unmask]>
Date:
Tue, 3 Oct 2006 11:12:51 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Wenger, George M." <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Wenger, George M." <[log in to unmask]>
Parts/Attachments:
text/plain (80 lines)
Dan,

Unfortunately the political reality today is that there are too many
politicians that don't represent the people who elected them, there are
too many that break laws simply because they feel they are politicians
and can get away with it, and there are too many whose moral values
don't reflect the office they were elected too.  I like you and many
others would rather be using SnPb solder as well as having good
politicians in government, but I certainly don't think that the
pragmatic solution is to look for how to live with Pb-Free solder and
bad politicians.  We should be saying the reality today (political or
not) is that there are lots of things that are wrong and our efforts
should be directed to what "can" be done not what "cannot" be done. 


Regards,
George
George M. Wenger
Reliability / FMA Engineer
Base Station and Subsystems Group
Andrew Corporation, 40 Technology Drive, Warren, NJ 07059 (908) 546-4531
[log in to unmask]

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Daniel Blass
Sent: Tuesday, October 03, 2006 10:35 AM
To: [log in to unmask]
Subject: Re: [TN] FW: [LF] RoHS Opposition (on Pb) isn't sound (SMT Sep
2006)

Inge,

We have plenty of negative data on lead-free, whether it is reliability
of the solder, IMC voiding on copper pads, mixing Pb and Pb-free solder,
PCB damage in Pb-free reflow, etc.  But our job is to be pragmatic, to
look for solutions and know what can and cannot be done.

I'd rather be using PbSn solder but that is not the political reality
today.

Daniel Blass
Process Research Engineer
Area Array Consortium
Advanced Process Laboratory
Unovis Solutions
Universal Instruments Corporation
Visit us on the web at www.unovis-solutions.com

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

------------------------------------------------------------------------------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.  
If you have received it in error, please notify the sender
immediately and delete the original.  Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------------------------------
[mf2]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2