TECHNET Archives

March 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Brian McCrory <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 22 Mar 2001 10:02:54 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (65 lines)
Emily Tse wrote:

> Dear TNers,
>
> My team is trying to carry out an experiment under IPC-TM-650-Test Methods
> Manual (number 2.3.24.1) -  a Porosity Testing of Gold Electrodeposited on a
> Nickel Plated Copper Substrate Electrograhpic Method.  The test is a bit
> outdated but it seems to fit the best in our evaluation at this stage.
>
> However, one of the materials required for the test is no longer available
> in the market (Kodabromide, glossy finish, single wt. photographic paper,
> fixed before use).  From the Kodak webpage, they have suggested another
> replacement of Kodabrome II RC Paper.  Yet the paper base has been changed
> from Fiber to RC.  Will that change the result of the test?
>
> We would also like to know if there is any amendment on the test (if I have
> missed!) as well as other possible replacement for this particular
> photographic paper.
>
> Looking forward for your kind suggestions!
>
> Best Regards,
>
> Emily Tse
> Process Development Engineering
> ASAT Ltd.
>
> ______________________________________________
> FREE Personalized Email at Mail.com
> Sign up at http://www.mail.com/?sr=signup
>

Emily,

You might want to get a copy of ASTM B 741, "Porosity in Gold Coatings on Metal Substrates by
Paper Electrography".  I don't have the latest version which I think is -95.  My copy of B
741-90 recommends "Kodak Dye Transfer Paper Grade FDW (Catalog No. 1455302)".   The ASTM
method also has several technical paper references on porosity testing.  I don't believe that
the current IPC-TM-650 test method is under review at this time.  It probably should be if we
(IPC) can find a task group with the expertise and is willing to undertake such a review.  I
don't personally have experience with this test.  Hope this helps.


--
Brian McCrory

Delsen Testing Laboratories, Inc.
1024 Grand Central Ave.
Glendale, CA  91201

Phone:  818 247 4106
FAX:    818 247 4537
email:  [log in to unmask]
URL:    http://www.delsen.com/

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2