TECHNET Archives

January 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jon McDowell <[log in to unmask]>
Date:
Mon, 30 Jan 2006 10:12:59 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Dehoyos, Ramon" <[log in to unmask]>
Parts/Attachments:
text/plain (86 lines)
        SAC305 means 96.5%Sn 3%Ag and 0.5%Cu so based on this type of
naming SAC95 would be:  86%Sn 9%Ag and 5%Cu very unlikely due to its
high melting temp. 
        Ramon 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jon McDowell
Sent: Monday, January 30, 2006 10:01 AM
To: [log in to unmask]
Subject: Re: [TN] Pansert AVKII through hole diameter?

 Group

My apologies, I meant SAC305 solder, I am not sure where I got SAC95
(does such a thing exist?).

Sorry about that.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jon McDowell
Sent: Friday, January 27, 2006 4:19 PM
To: [log in to unmask]
Subject: [TN] Pansert AVKII through hole diameter?

Hello group
 
My name is Jon McDowell, and I work as a Quality Technician at ECCO in
Boise ID. We manufacture back-up warning alarms for the auto/truck
industries.
 
I have a question for you.
 
We are using the Pansert AVKII through hole insertion machine, which
call out that the diameter for through holes be .020 larger than the
upper tolerance of the wire diameter being inserted in that hole.
However I have been informed that a hole which is .020 over the lead
diameter may cause problems with soldering, particularly with the SAC95
solder.  Can anyone advise on this.
 

Thank You
Jon McDowell
Electronic Controls Co (ECCO)
833 W Diamond St
Boise Id 83705
P 208 395-8025


 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2