TECHNET Archives

April 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"McMonagle, Michael R." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 22 Apr 1999 11:35:59 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (76 lines)
Jim,
        The best rule to use is that it's never safe, unless you're
properly grounded. ESD charges can be transmitted to components whether
they are alone, in an PCB, in a ESD bag or in a finished chassis
assembly. Handle everything with this attitude, and you should have no
problems. Don't let anyone try to get away with the other attitude of
'It's a passive component (resistor/cap/etc), so I don't need to be
protected". This implements a dual standard, and allows for people to
forget when they are handling ESD sensitive devices. Implement a
consistent, across the floor, ESD policy from the receiving dock all the
way through to the shipping dock, and enforce it mercilessly.

Mike McMonagle
PCA Process Engineering Supervisor
K*Tec Electronics
1111 Gillingham Lane
Sugar Land, TX  77478
(281) 243-5639 Phone
(281) 243-5539 Fax
[log in to unmask]

> -----Original Message-----
> From: West, Jim [SMTP:[log in to unmask]]
> Sent: Thursday, April 22, 1999 10:28 AM
> To:   [log in to unmask]
> Subject:      [TN] Boards sensitive to ESD
>
> Hello all,
>
> It seems to me that everyone may have a different opinion concerning
> the
> handling of ESD sensitive boards.  The questions that I ask people and
> the
> question that I get asked often is, when is the sensitive part safe.
> 1.
> After you attach to the board, 2. After you attach to the board and
> apply
> it's power source, 3. or after it is enclosed in it's housing or case?
> I
> have seen different answers from everyone even the ESD specialist like
> 3M.
> If anyone could add any insight I would really appreciate it.
>
> Thanks,
>
> Jim West
> Manufacturing Engineer
> PROMARK ELECTRONICS
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2