TECHNET Archives

April 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Phil Nutting <[log in to unmask]>
Date:
Tue, 9 Apr 2002 08:37:18 +0100
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "FOX, Ian (York Rd)" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"FOX, Ian (York Rd)" <[log in to unmask]>
Parts/Attachments:
text/plain (67 lines)
If you carry out weight loss trials you will find that temps above 105 degC
and dwells of approx 4 hours are required to fully remove moisture from
saturated PCB's, but in practice 2-2.5 hrs is usually sufficient to dry a
board prior to coating. These times and temps will not impact on the
reliability of product.

Ian Fox
TRW AS

-----Original Message-----
From: Phil Nutting [mailto:[log in to unmask]]
Sent: 08 April 2002 17:13
To: [log in to unmask]
Subject: [TN] Bake before Conformal Coat


Good day, Technet

After reviewing past threads regarding baking boards before conformal
coating I come up with quite a varied selection of ideas.
I found 1 hour @100°C, 4 hours at 150°C, and 4-5 hours at 125°C.
My design engineer is concerned about the boards being exposed to this
temperature for an extended time. Yes, in the wave solder it sees much
higher temperatures... for a short period of time.  Our aqueous wash system
dries at about 65°C for 20 minutes.
Our product normally is tested to 40 - 50°C depending on the customer needs.
The past threads suggested raising the temperature above 100°C to "boil off"
any remaining water.

Can this time/temperature be narrowed down any? 

And if we use a lower temperature are we possibly trapping moisture? 

How will the reliability be affected by these elevated temperatures.

Thanks in advance,

Phil Nutting

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/scripts/wa.exe?S1=technet
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2