James,
We normally look at the mfr's spec for the post. They may provide
recommendations for hole size and finish.
We have found that HASL works nice for press fit.
Other finishes might do better with a swage or flare termination.
-Carrie
-----Original Message-----
From: Cagle, James [mailto:[log in to unmask]]
Sent: Tuesday, October 07, 2003 11:49 AM
To: [log in to unmask]
Subject: [TN] 0.045 post hole size
We have boards that we are pressing 0.045 square post into and then solder
them. We are having problems with the gold finish boards (holes too small
and pads lifting). My question is their a specs or suggested guidelines as
to the drill size and plating thickness required.
>
> James Cagle
> Tyco Printed Circuit Group-Hayward Division
> email: [log in to unmask]
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|