TECHNET Archives

August 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stadem, Richard" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stadem, Richard
Date:
Wed, 10 Aug 2005 16:01:11 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (63 lines)
Well, Steve
I don't profess to know an awful lot about pwb manufacturing, but let me
just point out that tech sales people are only so good at selling,
products must sell themselves in order to survive in this industry.
Most OEMs and CEMs need to qualify processes. We don't just buy products
and bring them into our shops and hope for the best.
We are required to completely test out everything to make absolutely,
positively certain that the resulting product meets the specifications
fully. We do our best to derive evaluation plans and follow them. Most
of us have done this with immersion silver on our pwb's, and the pwb
suppliers have also done likewise. 
And immersion silver has done very well, as far as I have been involved.
And from what I see on the Technet, the same with others. As far as
ENIG, well there is enough documented evidence that it is not always the
best choice. And in certain cases, neither is immersion silver. As the
respected Doug Pauls has pointed out (altogether now, gang), It Depends.
I don't know anything about the cyanide and formaldehyde issues, so I
cannot comment on that. I am sure other PWB vendors can, and will. I
wonder why so many board fabricators are not having a problem offering
IS if there are problems with the waste stream as you state. Did
something happen such that your local controlling agency is deviating
from state and federal guidelines?

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Hodge
Sent: Wednesday, August 10, 2005 2:46 PM
To: [log in to unmask]
Subject: Re: [TN] RoHs board surface recommendations.

I realize that tech sales people have done their job promoting immersion
silver to end users. The people who bad-mouth ENIG have been sold a bill
of goods. Cyanide is bad I know. I have a question for the effluent
controlling agencies. Why is more Cyanide allowed in the stream than
Silver? Our local controlling agency will not allow our company to even
consider immersion silver. Companies that offer IS chemistry will not
tell you this of course. More research? Yes, they have alot of lost time
to make up.

Formaldehyde going away? Then what? Back to the Blackhole. LOL

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2