TECHNET Archives

November 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Joyce Koo <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Date:
Tue, 11 Nov 2008 22:57:29 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (73 lines)
Imag is. Chem process.  Control by solution composition, ph, etc.  It is self limiting. If done properly, it could be on site.  I did plate a copper coin using just the stuff your vendor mentioned.  However, I did check conc, ph, temp, surface cleanliness, etc.  Make sure he take the waste with him if you allow him to set a foot in your plant.  Good luck. 
--------------------------
Sent using BlackBerry


----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Tue Nov 11 22:46:51 2008
Subject: [TN] Repair to ImAg plating?

Hi everyone,

 

We have an issue with loss of plating adhesion on some ImAg finished PCBs.
The affected area is small and consistent in location across the PCBs with
the defect.  All other areas seem to be ok when tested per a tape test.  The
PCB supplier is proposing to visit and "repair" them here at our site.  I
was not even aware plating could be repaired, let alone away from a PCB fab
shop without plating lines etc.  Is this even possible?  I am very hesitant,
as I very seriously doubt the control and/or quality of the "repair"
process.  At the very least, how would thickness be controlled?  We specify
micro 5-12 inches in thickness per IPC-4553, and the overall PCB is to meet
IPC-6012 Class 3.

 

Anyway, they described the process as follows:

 

I will send you the solution by Fedex in a small bottle. Once you have
received it, I will come to your facility and repair the boards.  I will
need a hot plate and Pyrex container to heat-up the solution to 120 F. Do
you have these two items? Otherwise I will bring them with me. I will clean
and repair the boards locally.  Once it is done, I will do the tape test to
make sure the adhesion of the silver is adequate.

 

My little voice is screaming "NOOOOOOOOOOOOOOOOOOOOOOO!!"

 

Thanks in advance,

Kevin


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2