TECHNET Archives

January 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
quoted-printable
Sender:
Subject:
From:
Sheila Smith <[log in to unmask]>
Date:
Wed, 6 Jan 1999 10:59:44 -0500
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Sheila Smith <[log in to unmask]>
Parts/Attachments:
text/plain (39 lines)
Jim,  A "bond primer" is often used on phosphoric anodized aluminum surfaces prior to bonding, especially when the application is considered primary aircraft structure.  Depending on the cure temp of your epoxy resin (ie 250F or 350F), Cytec has several bond primers that you could use.  I have found, however, large minimum buy requirements and long lead times.  Also, most of these bond primers must be applied within 24 hours of anodizing ... not always easy to accomplish if you are using job shops for the process.  Cytec is @ 714-630-9400.

Feel free to contact me off line if you'd like more information.

Sheila Smith, Marconi AES

----------
From:  Jim Marsico 516-595-5879
Sent:  Wednesday, January 06, 1999 8:22 AM
To:  [log in to unmask]
Subject:  [TN] PHOSPHORIC ACID ANODIZE

We are considering phosphoric acid anodize treatment of a cast aluminum (A356 alloy) for a bonding process (polyimide PWBs to the aluminum core).  Would there be any benefit to having the aluminum primed after anodizing, or would the "as-anodized" surface be better for bonding?  How about shelf life?
Thanks in advance,
Jim Marsico

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2