TECHNET Archives

June 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Vanderhoof, Brad" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum." <[log in to unmask]>, "Vanderhoof, Brad" <[log in to unmask]>
Date:
Wed, 9 Jun 1999 09:17:54 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (82 lines)
If your product and business make this a viable option have the board fab
house do the sorting.  Otherwise the value chain looks like:
fab baords -- test boards -- mark X-outs -- mix X-outs into production --
ship to assembly house -- sort to segregate X-outs.

Regards,
Brad

-----Original Message-----
From: Jack Olson [mailto:[log in to unmask]]
Sent: Wednesday, June 09, 1999 8:49 AM
To: [log in to unmask]
Subject: Re: [TN] Marking bad boards?


We may be faced with a similar problem soon (installing an in-house line) so
I would like to hear what you guys do about x-outs too.

Why not just sort them out as you go, and then when you had a sufficient
quantity built up to make it worthwhile, de-panelize the good ones and run
them as a separate job?

Just a thought (from a new guy who don't know nothin'),
Jack

                -----Original Message-----

                From: TechNet [mailto:[log in to unmask]]On Behalf Of Matthew
Lamkin
                Sent: Wednesday, June 09, 1999 4:18 AM
                To: [log in to unmask]
                Subject: [TN] Marking bad boards?

                Currently we have no working method of telling our Quad 100
p&p machines
                that a board is bad & not to place
                components on it.
                We have tried placing white dots on the boards but its a bit
hit & miss,
                so we just refuse to use panels with bad boards in.
                This I know causes problems & a slight price rise due to the
                manufacturers waste.



################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2