Ivanoe,
Read "Soldering for Electronics" by Klein-Wassink. All of the
dissolution rates are in there at given temperatures. Excellent book,
and I refer to it almost on a weekly basis.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ivanoe Pedruzzi
Sent: Monday, January 16, 2006 4:38 AM
To: [log in to unmask]
Subject: [TN] Dissolution rates and solder paste selection
Back on dissolution metals in molten solder, I remember reading on an
e-mail the following dissolution rates:
Dissolution rates
Au = 117.9 u"/sec.
Ag = 43.6u"/sec.
Cu = 4.1 u"/sec.
Pd = 1.4 u"/sec.
Ni = 0.05u"/sec.
Pt = 0.01 u"/sec.
At which temperature of the molten solder these dissolution rates are
applicable?
If I use those numbers to set up the TIME ABOVE LIQUID temperature
profile in a reflow oven, I'm not doing anything but the right thing, am
I ?
I also remember reading something about flux in the solder paste that
should be able to withstand that change (either longer time, or higher
temp, or both).
Upon your experience, is that practical? I don't remember any solder
paste representative talking about "...this paste for this plating, that
paste for that plating...". Do you?
Thanks, Ivan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|