John Sater wrote:
>
> Hello all:
>
> We are going to evaluate a new type of liquid applicable primary etch
> resist. Unlike commonly used resists, this one swells in the developer
> solution and requires a mild scrubbing action to be completely
> removed. Moreover, it is detached as flakes, very much like in the
> stripper.
>
> My question to all: Is anyone aware of developing machine that can
> scrub the resist off the panel and also remove the flakes to avoid
> redeposition on the panel? Our search so far yielded nothing and we
> suspect that we might need a custom built machine.
>
> Thanks,
>
> J. Sater
>
> _________________________________________________________
> DO YOU YAHOO!?
> Get your free @yahoo.com address at http://mail.yahoo.com
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
To
John Sater,
This happens as residual s/m or dry film foot print or scum.
Assuming that you have nice control over exposure,developing, and
characterstics of material that you are using on consitent base,
This problem can be controlled by
1. Using high pressure rinse
2. Light micro-etch and high pressure rinse
3. Usning alumina-jet scrubber
4. Using acid cleaner and micro-etch
This is somewhat maerginal problem and can be controlled easily.
Wish you best of LUCK
Fulabhai Patel
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|