Hi Marco,
It does not matter what temperature or RH you choose for your plotter room,
conditioning room, yellow room, etc -- provided that the conditions are the
same in all areas where the film is handled and used; and the conditions in
these rooms are not changing. Pick conditions that are easy to control to
and comfortable to work in. The film does need to be pre-conditioned and
plotted at the same temperature and RH as the yellow room where it will be
used. Complete pre-conditioning requires 6-8 hours if you use a cabinet
designed to allow air to come into contact with both sides of the film
(open wire shelves - one sheet per shelf). It will take considerably
longer under other conditions. After post-processing conditioning requires
1-2 hours on open shelves.
Regards,
Bob Seyfert
Technical Manager - Phototools
DuPont Electronics
At 03:15 PM 8/6/98 -0400, you wrote:
>Hi everyone!
>
>I'm currently involved in the production of artwork for pcb manufacturing
>and one major problem that we have is film stability. To my knowledge, raw
>films have to be pre-stabilized before use and again stabilized after
>processing at constant RH and temp (usually 55% and 23C) for 2 to 4 hours.
>If RH or temp increases, the dimension increase and vice versa. But what
>if raw films are pre-stabilized at a lower RH (say 45%) and after
>processing these are stabilized also at the same RH. Will the film still
>experience shrinkage even if it was stabilized at constant RH? (Same
>question also for Temp)
>
>If anyone can help me with this one, I'd appreciate it. Thanks!
>
>Marco Biagtan
>Artwork Process
>NEC Components Philippines Inc.
>[log in to unmask]
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|