TECHNET Archives

October 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Chafin, Ken G." <[log in to unmask]>
Date:
Mon, 1 Oct 2007 21:57:39 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Hfjord <[log in to unmask]>
Subject:
From:
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (63 lines)
Depends...oh, sorry, someone had copyright on that..


We have skipped the microgram 'philosophy' . Instead, we perform the below
'reality' tests regularly:


http://www.ipc.org/4.0_Knowledge/4.1_Standards/test/2.6.13.pdf


Inge

-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Chafin, Ken G.
Skickat: den 1 oktober 2007 21:47
Till: [log in to unmask]
Ämne: [TN] Ionic Cleanliness

Does any IPC Standard recommend a minimal level of  PC Board, or PC
Assembly ionic cleanliness in terms of material per square unit of board
or assembly area?

E.g.   0.2 micrograms of sodium chloride equivalent per square
centimeter.

In IPC-A-600D, section 19.1 a solvent resistively value for an
IPC-TM-650 test is given (greater than 2 X 10 to power 6 ohm per
centimeter is recommended).

Even if an appropriate response to this question is complex can the
question itself be answered yes or no?

Thanks for any guidance. 



Kenneth Chafin


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2