Is there an allowable limit to the total halides in no clean solder paste in
PPM?  I am familiar with the copper mirror, silver chromate, and ion
chromatography tests but I do not know if there is a published limit in IPC,
J-STD, or Bellcore.
Thanks,
Denis

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2