TECHNET Archives

February 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Franklin D Asbell <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 10 Feb 2004 09:26:15 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (29 lines)
Wow, thats serious flaking/peeling.

Sue, what does the copper underneath these areas look like? The areas where
the mask came off, discoloration, residue, etc?

Do you have any bare boards remaining? Do you know the finished copper
weight of these boards? Was it print and etch by any chance?

It gives the appearance of poor surface treatment prior to mask; however,
I've never seen anything that severe before, even contaminated surfaces will
hold solder mask to a degree, if they happened to apply solder mask over
copper foil perhaps the much smoother surface would prevent adequate
adhesion of the mask...poor cure should also be consider...

All this is assuming you did not soak the boards in diesal fuel for 2 days
before processing them....(that...was a joke people, lighten up)

Franklin

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2