TECHNET Archives

March 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Marty W. Sheppard" <[log in to unmask]>
Date:
Mon, 26 Mar 2007 10:27:20 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, ekalgren <[log in to unmask]>
Subject:
From:
ekalgren <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (55 lines)
Try arlon or Rodgers.  If you look at the last valid QPL, you'll find that
both of these companies are/were qualified for GR7.  Customer service at
either should be able to narrow things down further.

Eric Kalgren
Electrical Engineer
Cobham Defense Electronic Systems 
Continental Microwave Division 
11 Continental Drive 
Exeter, NH  03833  USA
Tel:  603-775-5200  
Fax: 603-775-5201 
E-mail:[log in to unmask]  
Website:  http://www.cobhamdes.com
 
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Marty W. Sheppard
Sent: Monday, March 26, 2007 8:47 AM
To: [log in to unmask]
Subject: [TN] Approved Substitute for Mil-P-13949/7 (GR)

We have an old drawing that calls for the material to be:

MIL-P-13949/7 (non-woven glass (GR) and polytetrafluoroethlyene resisn) for 
MICROWAVE applications; p/n GRN0310B1/B1B1C

I cannot find a direct sub when looking through the IPC4101 slash sheet 
index.  Can anyone tell me what material is used today for this requirement?

Thanks.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2