TECHNET Archives

November 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 26 Nov 2013 11:17:46 -0800
Reply-To:
stephen gregory <[log in to unmask]>
Message-ID:
Subject:
From:
stephen gregory <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (140 lines)
Hi Andy,
 
I didn't receive the pictures. Could you try sending them again by replying to this message?
 
Steve
 

________________________________
 From: Andrzej Zielinski <[log in to unmask]>
To: [log in to unmask] 
Sent: Tuesday, November 26, 2013 10:59 AM
Subject: Re: [TN] Separation between the BGA sodler ball and pad on the PCB
  

Hi,

Have sent pictures to Steve Gregory. 
For sure this is not HIP as I already went through this issue mid this year. 

Not sure about nickel fracture. 
Hopefully we will see more from the pictures. 

Andy
Sent using BlackBerry®

-----Original Message-----
From: Joyce Koo <[log in to unmask]>
Sender: TechNet <[log in to unmask]>
Date: Tue, 26 Nov 2013 16:13:12 
To: <[log in to unmask]>
Reply-To: TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo
    <[log in to unmask]>
Subject: Re: [TN] Separation between the BGA sodler ball and pad on the PCB

Hop is my guess. Warpage...

Joyce Koo
Researcher
Materials Interconnect Lab
Office: (519) 888-7465 79945
BlackBerry: (226) 220-4760

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Tuesday, November 26, 2013 11:11 AM
To: [log in to unmask]
Subject: Re: [TN] Separation between the BGA sodler ball and pad on the PCB

Hi Andy - if you can send the pictures to Steve Gregory, he can post them 
so we can all view them. What you describe sounds like Head on Pillow or 
possibly Brittle Nickel Fracture but having the pictures will assist in 
making an accurate assessment. One action you can take that will be very 
informative is to run shadow moire on the BGA to measure how much warp 
happens during the reflow process. Excessive package warp could be the 
root cause of your issue.

Dave Hillman
Rockwell Collins
[log in to unmask]



From:   Andrzej Zielinski <[log in to unmask]>
To:     <[log in to unmask]>
Date:   11/26/2013 09:34 AM
Subject:        [TN] Separation between the BGA sodler ball and pad on the 
PCB
Sent by:        TechNet <[log in to unmask]>



Dear Colleagues ..

I am facing an issue with the BGA part where in three locations we found 
separation between the BGA solder balls and pads on the PCB (ENIG finish).
This condition was discovered during the cross-section that we have 
requested from our local lab.
I can share few pictures I have taken from our report (can't attach the 
whole document as this report is confidential to our business).

Basically this BGA is the plastic ACTEL package 896 pins, SAC305 finish, 
soldered with leaded process using 62Sn/36Pb/2Ag solder paste. Temperature 
was slightly elevated to accommodate SAC305 solder finish from the BGA 
package.

The separation condition we have observed was only found in location A1, 
A16 & T16 which are the corners of the BGA package. As well all 3 
separations occurred after the reflow process was completed because there 
is an evidence of completed inter-metallic fusion. 

In location A16 & T16 you can see the copper is protruding of the pad but 
I have been told this is not an issue and cause of the separation.
I was considering package or PCB warpage as the cause of this separation 
or something related to cooling the board after reflow.
I asked our lab to measure the height of the solder balls across row A & T 
and they all deem to be ok.
I have asked to check for the phosphorus content as the pad level to see 
if this is related to black-pad symptom and the phosphorus was measured as 
10.3%.

So far the board assembly house is adamant their reflow profile is 
correct.
PCB manufacturer is confident with their PCB and pointing to the assembly 
house.
There is a thought about poor sample preparation where the separation 
issue would be caused by the lab (during cross-section).

We are attempting to perform another cross-section on different board but 
here I am not really sure if this is the right way to go (extra cost).
Because I have never seen such a defect, I am not sure what should be the 
next step to take.
Any advice guys ?

Andy




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2