TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0uozRs-0000LMC; Fri, 9 Aug 96 16:50 CDT
References:
Date:
Fri, 9 Aug 1996 17:44:49 PST
Precedence:
list
Resent-From:
From [log in to unmask] Mon Aug 12 09:
22:10 1996
Message-ID:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/5687
TO:
Return-Path:
<TechNet-request>
X-Loop:
X-Juno-Line-Breaks:
0-10,12-36
Resent-Message-ID:
<"3MYoF1.0.t5J.ZAx2o"@ipc>
Subject:
From:
[log in to unmask] (John E Nelson)
Old-Return-Path:
Cc:
X-Mailer:
Juno 1.00
Resent-Sender:
TechNet-request [log in to unmask]
Parts/Attachments:
text/plain (47 lines)
In a previous life I tested several chemical pre-cleans for Vacrel and 
never was able to achieve the same adhesion as with mechanical scrub.  

The best comparison is done using a scratch test.  (works for LPI too).
Take a  sharp knife and cut  a cross-hatch pattern  into the mask of\ver 
a ground plane  area.  The mask should not chip back from the cut 
more than a few thousandths.  The test is subjective so run samples
of each of several cleaning processes and scratch them similarly 
and compare the relative amount of chipping.   You'll readily decide 
which process is best.
 
On Fri, 9 Aug 1996 10:23:53 -0500 "Todd Rogers" <[log in to unmask]>
writes:
>We are attempting to switch our pre-clean process prior to soldermask 
>from
>chem-clean followed by a mechanical scrub to chem-clean only.  We have
>experienced problems with poor soldermask adhesion at the nickel/gold 
>tab
>area.  We are using a reverse current tin/lead strip prior to 
>nickel/gold
>and the HCL seems to be getting under the mask causing it to peel.  
>Has
>anyone else had experience with a chem-clean process prior to 
>soldermask
>and reverse current plate prior to nickel/gold.
>
>***************************************************************************
>* TechNet mail list is provided as a service by IPC using SmartList 
>v3.05 *
>***************************************************************************
>* To unsubscribe from this list at any time, send a message to:        
>   *
>* [log in to unmask] with <subject: unsubscribe> and no text.     
>   *
>***************************************************************************
>
>

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2