TECHNET Archives

May 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Gary Bremer <[log in to unmask]>
Date:
Tue, 29 May 2007 21:07:52 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Subject:
From:
John Burke <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (69 lines)
Gary I am sure someone on the forum will reply but I just wanted to comment
on those PhD's............

Scared? Might be more like cautious - they perhaps know what it would cost
to get the Maytag repair man to do a site visit in deep
space...................

John

 
 
John Burke
 
(408) 515 4992

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gary Bremer
Sent: Tuesday, May 29, 2007 8:29 PM
To: [log in to unmask]
Subject: [TN] Exposed copper (space applications)

Where is it stated that the conductive pattern can not have any exposed 
copper on the vertical surfaces?  Is that any empirical data that supports a

failure mode if there is exposed copper on the vertical surfaces of a 
conductive pattern? I have searched MIL-STD-2000, NASA-STD-8739-2 and 
NASA-STD-8739-3 but can only find that it is allowed. Where I work those 
with PhD's worry about exposed copper on the vertical edges of the 
conductive patterns and are scared to allow to move forward because of 
possible failure modes with a deep space launch. For my limited knowledge of

metallurgy: after copper is exposed to moisture and oxygen, corrosion takes 
place only on the surface and does not migrate any further. I do have access

to NHB5300 to see if exposed copper was not allowed.


Gary Bremer

_________________________________________________________________
PC Magazine's 2007 editors' choice for best Web mail-award-winning Windows 
Live Hotmail. 
http://imagine-windowslive.com/hotmail/?locale=en-us&ocid=TXT_TAGHM_migratio
n_HM_mini_pcmag_0507

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2