TECHNET Archives

March 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 11 Mar 2003 08:14:00 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Yannick Brisson <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Yannick Brisson <[log in to unmask]>
Parts/Attachments:
text/plain (47 lines)
Hi, 

  We experience some void in BGA.  We try different paste and profile but
nothing seem to eliminate those void. We try something, we took a BGA and
put only  flux on the ball( Flux 297DX from AIM) and we didn't see any
voiding after that...

  We use stencil of .006mil, and .005mil of thickness, and we had some
medium to large void

  We also try a .004 stencil ( like a mini-stencil) where we put some paste
and we had some little BGA.

  My question is, could the paste and the ball of the BGA could not be
compatible( we use a no clean solder paste, 63/37, our Solder ball under BGA
are also 63/37).

  Or is the stencil thickness is very important??

  We use a 10% reduction on the stencil whti round pad

Thanks You

Yannick Brisson
============================
Technicien SMT
Technician SMT
M2S Électronique
2855, Rue de Celles 
Québec, Québec
G2C 1K7
Téléphone: (418) 842-1312 Ext: 264
Télécopie: (418) 842-0123
[log in to unmask]
============================

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2