TECHNET Archives

January 2018

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Guy Ramsey <[log in to unmask]>
Date:
Mon, 8 Jan 2018 11:19:22 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Roger Mack <[log in to unmask]>
Message-ID:
Subject:
From:
Roger Mack <[log in to unmask]>
Content-Type:
text/plain; charset="US-ASCII"
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
MIME-Version:
1.0
Parts/Attachments:
text/plain (62 lines)
We have spent a lot of time on this also. We do x-ray everything inline 
and have adopted 50% as the void limit for the cooling plates of QFN's as 
our default in workmanship. Heat transfer requirements of the part may 
require tighter limits and be documented for that product.

We epoxy fill and plate over all vias in the cooling plate, so unlike the 
photo on page 18 - no open vias.

We have had great success with the solid pad and print area is key. You 
want to cover about 60% to 70% of the area to keep the void area safely 
below you limit. The suggested stencil picture on page 17 may work, but 
with that many grids it is tough to get a coverage of around 60% to 70%. 
For most smaller QFN's a grid of 2 x2 works best for us. It is best to 
test the stencil apertures as this must also work with the amount printed 
on the signal pins.

Make sure QFN voids like this aren't actually insufficient print coverage.



Roger Mack  P.Eng. 
Manufacturing Specialist
Parker Hannifin Canada
Electronic Controls Division
1305 Clarence Avenue
Winnipeg, MB  R3T 1T4 Canada 
direct 204 453 3339 x7373
[log in to unmask]
www.parker.com/ecd







From:   Guy Ramsey <[log in to unmask]>
To:     <[log in to unmask]>
Date:   2018-01-08 10:26 AM
Subject:        [TN] solder voids - QFN belly pad
Sent by:        TechNet <[log in to unmask]>



We are having trouble with a lot of boards.
We are seeing excessive voids like the ones on page 18 of this
presentation.

https://urldefense.proofpoint.com/v2/url?u=https-3A__www.google.com_url-3Fsa-3Dt-26rct-3Dj-26q-3D-26esrc-3Ds-26source-3Dweb-26cd-3D1-26ved-3D0ahUKEwj27JnJ38HYAhUF5YMKHWYICvcQFggpMAA-26url-3Dhttps-253A-252F-252Fwww.eptac.com-252Fwp-2Dcontent-252Fuploads-252F2012-252F06-252Feptac-5F07-5F18-5F12.pdf-26usg-3DAOvVaw2OX6J-5FYRqkuNUNNgDBvmwZ&d=DwIBaQ&c=zQLjxGaFENyz7VqOLRV_eQ&r=MTRQzKHrCCjgWzO_2fNMPjXUAeXe2IKt2DAIM9Q7PbA&m=HTryF-M_lvSHzqCszzIZ_UKKoCa9tYeOlDa0ngUHuZ8&s=8SAYbi6rfvdeiLoHzWO9k2YQqKHTv0AFJxCuknKLZc4&e=



The vias are filled and plated. Anyone seen this, resolved it?


Guy



llllllllllllllllllllllllllllllllllllllllllllllllllllllllllllllllllllll
"PLEASE NOTE: The preceding information may be confidential or privileged. It only should be used or disseminated for the purpose of conducting business with Parker. If you are not an intended recipient, please notify the sender by replying to this message and then delete the information from your system. Thank you for your cooperation."