We tried it as a replement to Humiseal 1b31. We found that It has a better adhesion then the Humiseal and it is cheaper. But, we did not continue to evaluet it. IPC 830 deal with conformal coating.
Gil Zilber,
Elta Systems
-------- הודעה מקורית --------
מאת: Victor Hernandez
תאריך:20/06/2014 3:46 PM (GMT+02:00)
אל: [log in to unmask]
נושא: Re: [TN] Conformal Coating
Fellow TechNetters:
I have not received many responses to my conformal coating inquiry, ACCL-53T. Perhaps someone can share parameters associated with the process such as application equipment, spray nozzle, thickness, Drying, coverage, etc. Is there an associated IPC Standard that I can review?
I would very much appreciate any information you can share.
Victor,
From: Hernandez, Victor G
Sent: Wednesday, June 18, 2014 8:03 AM
To: Stadem, Richard D.; TechNet E-Mail Forum
Cc: Hernandez, Victor G
Subject: RE: Conformal Coating, ACCL-53T
Good response for SAFETY, but searching for something more constructive with regards to the above stated product..
Victor,
-----Original Message-----
From: Stadem, Richard D. [mailto:[log in to unmask]]
Sent: Tuesday, June 17, 2014 3:47 PM
To: TechNet E-Mail Forum; Hernandez, Victor G
Subject: RE: Conformal Coating
Yes, acceleration to 53 mph, tops, has always been a safe way to drive.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Tuesday, June 17, 2014 3:01 PM
To: [log in to unmask]<mailto:[log in to unmask]>
Subject: [TN] Conformal Coating
Fellow TechNetters:
Anyone out there has experience with ACCL-53T?
Victor,
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
The information contained in this communication is proprietary to Israel Aerospace Industries Ltd. and/or third parties, may contain confidential or privileged information, and is intended only for the use of the intended addresse thereof. If you are not the intended addressee, please be aware that any use, disclosure, distribution and/or copying of this communication is strictly prohibited. If you receive this communication in error, please notify the sender immediately and delete it from your computer.
Thank you.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|