We had an oil contamination (actually too much wave oil) in our pot and used
a simple techique of collecting it on a paper towel floated on top of pot
while wave was running for a brief period (note that too long and the paper
could ignite...)
Bottom line though, if pot is stirred (by running wave) then wave shut down
the particles (being lighter than solder...) will float and removing dross
should do it. I'ld repeat 2-3 times and then you could I suppose check the
dross for contaminates....
Jim
-----Original Message-----
From: Michael Bell [mailto:[log in to unmask]]
Sent: Thursday, July 18, 2002 7:37 PM
To: [log in to unmask]
Subject: [TN] Solder Pot Contamination
Hi all,
Has anyone ever come across a method in which to detect resin (polyurethane
particles) contamination in a Wave Solder Pot???? And in turn, a method to
remove this sort of contamination???
Cheers
Mike
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|