Valquirio, you've noted an important issue before beginning your
experiment: what is the measure of performance? The uncertainty (quality)
of the measurement will affect something that you haven't mentioned: the
number of replications of each element in the L9 array. Lou Hart
-----Original Message-----
From: Valquirio N. Carvalho [SMTP:[log in to unmask]]
Sent: Monday, April 01, 2002 8:42 PM
To: [log in to unmask]
Subject: [TN] Indium Solder
Hello Technetters:
I'm trying to develop and optimize a process for the following:
SMT part where the bottom of the device (gold over nickel) will be
soldered to a gold-plated copper surface (50-150 uin Ni, 3-8 uin Au)
below
the top of the board surface.
The copper surface is actually a "coin". The pcb is milled from the
bottom-side to a specific ground plane. The coin is then hi-temp
soldered (Sn95Sb) to the ground plane layer (this is done at the board
fab. shop).
The manufacturer of the smt part recommends a pure indium foil .25" x
.25",
.003" thick.
The component also has about thirteen gull-wing leads that depending on
the
tolerance stack-up, may be reflow soldered or hand soldered.
We're going to run three replications of an L9 DoE (four factors, three
levels) to develop and optimize the process.
So, several questions:
Where I'm soldering two gold surfaces, and low-temp is recommended, is
indium the best choice?
Any suggestions on how to evaluate the results of the DoE? X-Ray,
cross-sections, pull-tests, cleanliness?
Thanks for any input,
Valquirio N. Carvalho
------------------------------------------------------------------------
---------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
------------------------------------------------------------------------
---------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|