TECHNET Archives

January 2019

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Richard Kraszewski <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Date:
Sat, 5 Jan 2019 17:14:43 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (17 lines)
Two parylene coating  related questions regarding primers:

#1 - What is  the maximum time you would allow between priming and depositing  the parylene?

#2 - I have been lead to believe that if you place primer on an already coated parylene surface , the primer will act as a release agent for the next layer of parylene.   Better not to  add primer in this case but rather recoat ASAP.  Would welcome any and all thoughts. 

Thanks in advance 

Rich  Kraszewski 
Senior Staff Process Engineer
Plexus 


* * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *

This e-mail and any attachments are confidential from Plexus Corp. and may contain information which is privileged, confidential, and/or protected by non-disclosure agreements.  They are intended solely for the use of the named addressee(s).  .  Any unauthorized use or disclosure may be unlawful.  If you are not a named addressee, you must not use, disclose, retain or reproduce all or any part of the information contained in this e-mail or any attachments If you have received this transmission in error, please destroy it and notify us immediately by return e-mail or by calling + 1 888 208 9005.