TECHNET Archives

October 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Paul Signorelli <[log in to unmask]>
Date:
Mon, 8 Oct 2001 11:54:20 -0500
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (20 lines)
Bill,
The Thermal Shock of freeze mist can stimulate or cause a crack of a marginal BGA ball but
the main concern i would have is that the Freeze Mist will cause water to condense out
of the atmosphere. The condensed water will create an electrolyte and, assuming you
are doing this with the power on the board, you will grow dendrites under the BGA and this will cause shorts on high Z lines. This will cause masking of the original defect.
Any 'power on' cold temperature testing that causes the board to go through the dew point should be avoided.
See IPC-TR-476, Sandia Labs Report SAND 75-0616, Aerospace Report TOR-0075, NASA CR-61194, MSFC Alert MSFC-68-8, GSFC Failure analysis FAR10-012 and 1160,
for additional info on the hazards of electrochemical migration and dendritic growth on PCBA's.
Paul Signorelli

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2