> Dear friends,
>
> I'm interested in a method of creating "keep out" areas on my PWB
> designs which identify those locations not to be conformally coated.
>
> Some have suggested creating a silk screen on the PWB, some
> dimensioning it on the assembly drawing, others similar yet equally as
> difficult to change processes.
>
> Has anyone devised a method to accomplish this without the rework
> problems that are associated with change orders (i.e. obliterating
> silk-screen and remarking, changing assembly drawings, etc.)?
>
> Is there a reworkable or peelable solder mask (type) of material that
> can be easily applied to assemblies at any level then be removed prior
> to installation of the PWB into the box/rack/chassis?
>
> Thanks much, Rich.
> 310-364-9862
> [log in to unmask]
> [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################With respect to peelable soldermasks, a company named Lackwerke Peters
has developed and markets a peelable mask.
Let me know if youn require any further information.
Best regards,
Mike Carano
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|