TECHNET Archives

December 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Date:
Fri, 12 Dec 2003 08:30:53 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Steve Kelly <[log in to unmask]>
Subject:
From:
Steve Kelly <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (49 lines)
Hi Rudy'
It is a Type III Grade A gold per MIL-G-45204 - 99.9% pure, knoop less than
90. Regards Steve Kelly

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Rudy Sedlak
Sent: Thursday, December 11, 2003 6:24 PM
To: [log in to unmask]
Subject: Re: [TN] Cleaning of Wire Bondable Gold

Steve:

I suspect you are not plating a pure gold, but a "hard gold", which means an
alloy...and the alloy metal is oxidizing...

Given that, a mild acid should be ideal...suspect a citric acid based
product
would clean things up nicely.

If you have problems with the matter, contact me directly, I am sure we can
find something that will do the job easily.

Rudy Sedlak
RD Chemical Company

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2