TECHNET Archives

November 2017

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
David Hillman <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 17 Nov 2017 15:54:29 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Giamis, Andy" <[log in to unmask]>
Message-ID:
Subject:
From:
"Giamis, Andy" <[log in to unmask]>
Content-Transfer-Encoding:
base64
In-Reply-To:
Content-Type:
text/plain; charset="utf-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (1 lines)
Thank you all.



From: David Hillman [mailto:[log in to unmask]]

Sent: Friday, November 17, 2017 6:10 AM

To: TechNet E-Mail Forum <[log in to unmask]>; Giamis, Andy <[log in to unmask]>

Subject: Re: [TN] Dissolution rates of noble metals in tin



Email Security Warning:





The following message was sent from an external e-mail address. Exercise caution when opening attachments, clicking links, or exchanging information.





Hi Andy - I have some stuff in my files which I'll send you once I get to the office (first part of today is a Rockwell Roadshow where we feed LN2 frozen marsh mellows to students and other fun science stuff!). Do a search for Wally Bader's classic dissolution work - its for tin/lead and not tin but it would give you a pretty good first order estimate. Also look in the American Welding Society (AWS) Soldering Handbook - I believe Paul Vianco has data in that reference. Is there a specific noble metal of interest?



Dave Hillman

Rockwell Collins

[log in to unmask]<mailto:[log in to unmask]>



On Thu, Nov 16, 2017 at 10:48 PM, Giamis, Andy <[log in to unmask]<mailto:[log in to unmask]>> wrote:

I’m looking for a reference showing the dissolution rates and temperature dependence of noble metals in tin.



A wise man (wise guy, AKA George) used to always carry two things: an IKEA measuring tape and a great chart showing this data.



I’ve searched Wikigooglepedia and have been through my 2006 CRC handbook (Phys and Chem) and several solid state texts.



Thanks

Andy