TECHNET Archives

December 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Pete Houwen <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Pete Houwen <[log in to unmask]>
Date:
Mon, 1 Dec 2008 08:29:19 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (32 lines)
Henry,

"Apparently the plating committee and the enig suppliers have been looking at 
this and it is described as a bit of an epidemic and they are calling it a new 
phenomenon that could rival black pad. "

Applying the common sense test, if this is a phenomenon due to the ENiG/lead 
free wave, why is it new, only appearing now?  These processes have been in 
place for years, something has to have changed to start this epidemic.  (we 
could blame it on global warming!)  Black pad didn't start off small and spread 
into an epidemic.  It just was.

So, since the technology is stable, look at the process at the fabricator or 
assembler.

"We are seeing everything in spec from the board vendors (thickness/P 
content) "

Is this based on your testing or their reports?  I've got a report right here 
showing boards passing with flying colors, and independent microsections and 
XRF that tells a very different story.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2