Leif,
Are the contacts coming loose from the housing/body or on the board?
You describe warping and twisting of the connector; what is the
specified reflow heat capacity of that connector? It seems to me that
the temp at the board is exceeding the limits of the connector body
material.
Doug Erb
Senior FAE
Hirose USA
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier /*
Sent: Friday, May 15, 2009 2:22 PM
To: [log in to unmask]
Subject: Re: [TN] Connector with loose pins
Hi Leif
You do not say how long that connector is and what the connector body
material is.
My guess on very skimpy info is that you have a too long connector made
with an unsuitable connector body material, with connector pins made of
some connector pin metal, like BeCu, that while it is a good connector
pin material with good spring characteristcs, it makes for bad solder
joints
Werner
-----Original Message-----
From: Leif Erik Laerum <[log in to unmask]>
To: [log in to unmask]
Sent: Fri, 15 May 2009 5:16 pm
Subject: [TN] Connector with loose pins
Technetters,?
?
I have a less scientific question, but I hope someone has some
experience with a similar problem.?
?
We have a .090 think motherboard where one particular part number
connector frequently have loose pins. It is 33 cm by 16mm. There are
lots of other types of connectors on the board that does not have
issues. We only have problem with one part number. These connectors are
at the very front of the board. They go in the oven first. This is a
leaded solder board and we use SN63/Pb37 solder. The loose pins tend to
be at the end of the connector and on power planes. On some boards it
appears that the connector sort of twists or bows a little bit.?
?
The problem is that this surface mount connector is very hard to fix.
The pins frequently short and due to space limitations, it is hard to
reach them with the tip of the soldering iron. They also tend to develop
shorts easy. This makes it even harder to fix after reflow.?
?
We have tried reducing the cooling at the end. We have sent the boards
through the oven with the mate installed in order to stiffen up the
connector. The profile was checked as late as today. Nothing jumped out
at me.?
?
Does anyone have experience with a similar problem that they managed to
solve??
?
Thank you.?
?
--
Leif Erik Laerum?
?
---------------------------------------------------?
Technet Mail List provided as a service by IPC using LISTSERV 15.0?
To unsubscribe, send a message to [log in to unmask] with following text
in?
the BODY (NOT the subject field): SIGNOFF Technet?
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)?
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest?
Search the archives of previous posts at:
http://listserv.ipc.org/archives?
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815?
-----------------------------------------------------?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|