TECHNET Archives

May 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Tue, 25 May 1999 05:33:43 -0700
Reply-To:
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
Organization:
SP Precision
From:
Eric Miller <[log in to unmask]>
Parts/Attachments:
text/plain (73 lines)
Hi Kat, I would steer you away from the water soluble mask, it has the
tendency to clog Filters in the water purification system. Ted made a
suggestion to use a peelable mask instead of a water soluble mask, good
suggestion! But this also calculates into labor in a production
environment. Now my two cent's worth, use a fixture or pallet to mask off
any given area's of a circuit board!  The fixture will mask off bottom side
smd's, while exposing only the parts that need to be waved. It's a fast and
simple solution to a majority of mixed tech PCB's. This will decrease the
labor that is involved with the manufacturing of the circuit card, and,
increase the through put through the wave solder line! If you need any
help, give me a call off line.
Eric Miller
S.P.P.I.
800-725-5388

-----Original Message-----
From:   Kat Lee [SMTP:[log in to unmask]]
Sent:   Tuesday, May 25, 1999 2:50 AM
To:     [log in to unmask]
Subject:        [TN] Plated Through-Hole

Hello everybody,
This is my first time mailing to the list.

I'll get straight to the point - you see, a product of my company has a
plated through-hole that must not be soldered.
The past solution was to cover the whole thing with a kapton tape before
running it through the wave. Now we have suggestions of using a plug or
water-soluble masking tape.
I was wondering if any of you have any experience in this matter and could
share anything with me.

Thanks in advance.

Kat LEE

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2